• Homebuilt Airplanes is a vibrant community of pilots, plane builders and industry experts. Our thousands of active members use HBA to trade detailed technical information, discuss best practices, share their builds, plan get-togethers and buy/sell planes & parts. In addition to the community you gain access to, you gain access to over 20 years of curated knowledge by some of the brighest in the industry.

    Access to HBA is subscription based. It is free for 7 days so you can get to know our community!

    Click Here to Become a Member and Access HBA

Galvanic corrosion

Joerg989

Member
Joined
Mar 28, 2023
Messages
5
Location
Germany
To prevent electrochemical corrosion between aluminum and carbon, I typically use layers of glass cloth for insulation. Is this still necessary after the aluminum parts have been treated with Alodine?
 